Platinum-cure PSAs (2013, 7657, 7659 with Syl-Off 4000 Catalyst) are two-part systems with a bath life of 24 hours or less at 21 °C, cure at as low as 80 °C in a single-zone oven, and suit temperature-sensitive substrates, but the catalyst can be contaminated by peroxides and other materials. Peroxide-cure PSAs are one-part, have extended bath life, generally need >150 °C and a multi-zone oven for tapes, and are a robust cure system resistant to catalyst poisoning.
Table 1. Peroxide- vs. Platinum-Cure PSAs
| Platinum-Cure | Peroxide-Cure | |
|---|---|---|
| Dow Corning® brand silicone PSAs | 2013 Adhesive, 7657 Adhesive, 7659 Adhesive (with Syl-Off® 4000 Catalyst) | 280A, 282, 7355, 7356, 7358, Q2-7406, Q2-7566, Q2-7735 Adhesive |
| Components | Two-part system: silicone resin, crosslinker and polymer dispersed in solvent + platinum catalyst; catalyst required; 2013 Adhesive does not contain solvent. | One-part system: silicone resin and polymer dispersed in solvent; used with a peroxide curing agent. |
| Bath life | Generally 24 hours or less at 21 °C (70 °F) | Extended bath life |
| Cure temperature and oven requirements | Can be cured at temperatures as low as 80 °C (176 °F) in a single-zone oven. | For tape constructions, cure temperatures >150 °C (302 °F) are generally required; cure is a two-step process that requires a multi-zone oven. |
| Benefits | Fast, low-temperature cure; may be used on temperature-sensitive substrates. | Robust cure system; catalyst resistant to poisoning. Adhesive properties may be modified by manipulating peroxide levels and oven conditions. |
| Drawbacks | Platinum catalyst is subject to contamination by peroxides and other materials. | Failure to remove solvent can result in bubbling, low adhesion, low cohesive strength. Failure to adequately degrade the peroxide can result in “snow” crystals, instability in high-temperature applications. |
Frequently asked questions
What is the bath life of platinum-cure silicone PSAs?
Generally 24 hours or less at 21 °C (70 °F), so the coating bath should be used within 24 hours of catalyst addition.
What is the main drawback of peroxide cure?
Residual solvent causes bubbling and low adhesion/cohesion; incomplete peroxide breakdown leaves “snow” crystals and instability at high temperature.
This page is based on the following document. Values are typical, not specifications; verify with the original and product data sheets before design or purchase.
Dow, “Silicone PSAs for High Performance Selection Guide”, Form No. 30-1315-01-0524 S2D, © 2024 The Dow Chemical Company (2024 최신판); Dow Corning, “Product Selection and Application Guide — Dow Corning® brand High-Performance Silicone PSAs”, Form No. 30-083B-01 (AGP7825), ©2001, 2006 Dow Corning Corporation (2006 구판). 한국어 번역·정리: 한국건설트레이딩(KCT)
Suggested citation: “Peroxide-Cure vs. Platinum-Cure Silicone PSAs (Table 1)”, Korea Construction Trading (KCT) Technical Information, https://kconstrade.com/ja/technical/psa/platinum-vs-peroxide
More technical resources
For DOWSIL™ silicone selection, quotations and technical advice, please contact Korea Construction Trading. We do our best to support you technically, from product selection to process-condition review and troubleshooting. Technical support details →